La0.7Sr0.3MnO3/SrTiO3-(001) Heterostructure Formula: La0.7Sr0.3MnO3 Core Loss

Submitted by magnunor, February 10, 2016.

Author Comments: 35 nm La0.7Sr0.3MnO3 thin film grown epitaxially on a SrTiO3 substrate using PLD, acquired from the middle of film.

Register / log in to set favourite spectra and overlay plots.
loading plot..

You can manually set the axis limits.

Spectrum Metadata

Specimen Name
FEI Titan 80-300ST
Spectrum Type
Core Loss
Specimen Formula
La0.7Sr0.3MnO3
Data Range
628.4 eV - 682.4 eV
Elemental Edges
Mn_L2,3
Associated Spectra
CL La0.7Sr0.3MnO3/SrTiO3-(001) heterostructure, oxygen vacancies
CL La0.7Sr0.3MnO3/SrTiO3-(001) heterostructure, brown millerite oxygen vacancies
CL La0.7Sr0.3MnO3/SrTiO3-(001) Heterostructure
Microscope Name / Model
FEI Titan 80-300ST
Gun Type
Field Emission Gun
Incident Beam Energy
300 kV
Resolution
1.0 eV
Monochromated
No
Dispersion
0.2 eV/pixel
Convergence Semi-angle
24.2 mrad
Collection Semi-angle
33.1 mrad
Detector
GIF
Dark Current Correction
No
Gain Variation Spectrum
No
Calibration
zero + dispersion
Reference
M. Nord, P. E. Vullum, M. Moreau, J. E. Boschker, S. M. Selbach, R. Holmestad, T. Tybell (2015). Structural phases driven by oxygen vacancies at the La0.7Sr0.3MnO3/SrTiO3 hetero-interface Appl. Phys. Lett. 106:4 041604
DOI
10.1063/1.4906920
Reference URL
http://dx.doi.org/10.1063/1.4906920