LaS(Se)-TaS2(Se) Misfit Nanotube Formula: LaS(Se)-TaS2(Se) Core Loss

Submitted by Luc Lajaunie, January 15, 2018.

Register / log in to set favourite spectra and overlay plots.
loading plot..

You can manually set the axis limits.

Spectrum Metadata

Specimen Name
FEI Titan Low-Base
Spectrum Type
Core Loss
Specimen Formula
LaS(Se)-TaS2(Se)
Data Range
524.83 eV - 2008.05 eV
Elemental Edges
Se_L2,3, Se_L1, La_M4,5, Ta_M4,5
Microscope Name / Model
FEI Titan Low-Base
Gun Type
X-FEG
Incident Beam Energy
200 kV
Resolution
2 eV
Monochromated
No
Dispersion
0.726 eV/pixel
Acquisition Mode
stem
Convergence Semi-angle
18 mrad
Collection Semi-angle
25 mrad
Detector
Gatan Tridiem ESR 865
Dark Current Correction
No
Gain Variation Spectrum
No
Calibration
low loss + drift tube
Reference
Luc Lajaunie, Gal Radovsky, Reshef Tenne, Raul Arenal (2017). Quaternary Chalcogenide-Based Misfit Nanotubes LnS(Se)-TaS(Se)2 (Ln = La, Ce, Nd, and Ho): Synthesis and Atomic Structural Studies Inorganic Chemistry
DOI
10.1021/acs.inorgchem.7b02680
Reference URL
http://dx.doi.org/10.1021/acs.inorgchem.7b02680