Silicon Carbide 6H(hexagonal) Formula: SiC(6H) Core Loss

Submitted by Sylvie Schamm, April 29, 2005.

Source / Purity: Single crystal

Author Comments: Biblio cited in "Reference" for calibration purpose same spectrum before deconvolution is also proposed in this database Analyst: S.Schamm. Temperature: Room.

Register / log in to set favourite spectra and overlay plots.
loading plot..

You can manually set the axis limits.

Spectrum Metadata

Specimen Name
CM30
Spectrum Type
Core Loss
Specimen Formula
SiC(6H)
Data Range
90.31 eV - 173.51 eV
Source and Purity
single crystal
Elemental Edges
Si_L2,3
Keywords
imported from old site
Alternative URL
Old EELS DB
Microscope Name / Model
CM30
Gun Type
LaB6
Incident Beam Energy
100 kV
Resolution
1 eV
Dispersion
0.2 eV/pixel
Acquisition Mode
Diffraction
Convergence Semi-angle
8.4 mrad
Collection Semi-angle
10 mrad
Detector
Parallel: 666 Gatan
Dark Current Correction
No
Gain Variation Spectrum
No
Relative Thickness
0.4 t/λ
Reference
W.M. Skiff, R.W. Carpenter, S.H; Lin, J. Appl. Phys. 58(9) (1985) 3463-3469