ZrO2 Formula: ZrO2 Core Loss

Submitted by Ian MacLaren, July 5, 2017.

Source / Purity: Oxidised Zircaloy-4 in monoclinic form of ZrO2

Author Comments: Plotted as absolute differential cross section in barns.

Register / log in to set favourite spectra and overlay plots.
loading plot..

You can manually set the axis limits.

Spectrum Metadata

Specimen Name
JEOL ARM200F
Spectrum Type
Core Loss
Specimen Formula
ZrO2
Data Range
1802.53 eV - 3849.53 eV
Source and Purity
oxidised Zircaloy-4 in monoclinic form of ZrO2
Elemental Edges
Zr_L1, Zr_L2,3
Associated Spectra
CL Zr
Microscope Name / Model
JEOL ARM200F
Gun Type
CFEG
Incident Beam Energy
200 kV
Resolution
0.5 eV
Monochromated
No
Dispersion
1 eV/pixel
Convergence Semi-angle
29 mrad
Collection Semi-angle
36 mrad
Probe Size
.04 nm2
Integration Time
100 secs
Detector
GIF Quantum ER
Dark Current Correction
Yes
Gain Variation Spectrum
Yes
Calibration
Low loss + drift tube
Relative Thickness
0.32 t/λ
Deconvolutions
Fourier-ratio